Thermal Properties Metric English Comments
Specific Heat Capacity 1.28 J/g-°C
0.306 BTU/lb-°F
LG Chemical Phenol
Structure & Characteristics: C6H5OH. Phenol is a white crystalline solid with a distinct smellUses: Raw material of phenolic resins, dye stuffs, synthetic fibers, herbicides, photo material, aromati..
Specific Heat Capacity 1.28 - 1.73 J/g-°C

@Temperature 50.0 - 200 °C
0.306 - 0.413 BTU/lb-°F

@Temperature 122 - 392 °F
Average value: 1.50 J/g-°C Grade Count:2
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..