Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.129 J/g-°C @Temperature 1000 °C |
0.2697 BTU/lb-°F @Temperature 1830 °F |
|
Chosun Refractories 1600HA BOARD Board Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Specific Heat Capacity | 1.129 J/g-°C @Temperature 1000 °C |
0.2697 BTU/lb-°F @Temperature 1830 °F |
|
Chosun Refractories 1700 HA BOARD Board Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |