Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.038 J/g-°C | 0.2481 BTU/lb-°F | Liquid |
3M Fluorinert™ FC-770 Electronic Liquid 3M™ Fluorinert™ Liquid FC-770 is a non-conductive, thermally and chemically stable fluid with a wide liquid range (-125 to 95 deg C) for use in many low temperature heat transfer application such .. |