Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.219 J/g-°C @Temperature 20.0 °C |
0.0523 BTU/lb-°F @Temperature 68.0 °F |
|
Hogen Duralloy H3W 68 Tungsten/32 Copper PM Metal Composite RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is .. |