Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.214 J/g-°C @Temperature 20.0 °C |
0.0511 BTU/lb-°F @Temperature 68.0 °F |
|
Hogen Durakut H15W 68 Tungsten/32 Copper PM Metal Composite RWMA Class ECM-EDMDURAKUT Copper-Tungsten and Silver-Tungsten are manufactured as electrode materials for EDM (Electrical Discharge Machining), ECM (Electro Chemical Machining) and ECD (Electro Che.. |
|||
Specific Heat Capacity | 0.214 J/g-°C @Temperature 20.0 °C |
0.0511 BTU/lb-°F @Temperature 68.0 °F |
|
Hogen Duralloy H5W 70 Tungsten/30 Copper PM Metal Composite RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is .. |