Polymer Property : Specific Heat Capacity = 0.212 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.885 J/g-°C
0.212 BTU/lb-°F
ASTM E1269
CoorsTek Zirconia-Toughened Alumina, ZTA
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..