Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.831 J/g-°C | 0.199 BTU/lb-°F | |
MMCC Aluminum/Al2O3 55p Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |