Thermal Properties Metric English Comments
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novacite® 1250 Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novacite® 200 Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novacite® 325 Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novacite® Daper Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novacite® L-207A Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novacite® L-337 Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novakup® 1250 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novakup® 200 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novakup® 325 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novakup® Daper Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novakup® L-207A Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Specific Heat Capacity 0.803 J/g-°C

@Temperature 0.000 - 200 °C
0.192 BTU/lb-°F

@Temperature 32.0 - 392 °F
Typical Novacite; finer grades are lower than coarser grades
Malvern Minerals Novakup® L-337 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Specific Heat Capacity 0.803 J/g-°C
0.192 BTU/lb-°F
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..