Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.188 J/g-°C @Temperature 20.0 °C |
0.0449 BTU/lb-°F @Temperature 68.0 °F |
|
Hogen Duralloy H30W 80 Tungsten/20 Copper PM Metal Composite RWMA Class 12.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 material is .. |
|||
Specific Heat Capacity | 0.188 J/g-°C | 0.0449 BTU/lb-°F | Liquid |
Indium Corp. Indalloy 140 Bismuth Solder Alloy Information Provided by Indium Corporation |