Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.737 J/g-°C | 0.176 BTU/lb-°F | |
UBE Tyranno Grade S Ceramic High Temperature Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Specific Heat Capacity | 0.738 J/g-°C | 0.176 BTU/lb-°F | |
CeramTec Alunit® HS Aluminum Nitride Alunit® HS offers an extremely high thermal conductivity of 170 W/mK and outstanding electrical insulation properties. The thermal expansion coefficient of this material is comparable to silicon. I.. |
|||
Specific Heat Capacity | 0.735 J/g-°C | 0.176 BTU/lb-°F | |
UBE Tyranno Grade LoxM Ceramic High Temperature Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Specific Heat Capacity | 0.738 J/g-°C | 0.176 BTU/lb-°F | |
CeramTec CeramCool® Alunit® Aluminum Nitride CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |