Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.172 J/g-°C | 0.0410 BTU/lb-°F | |
Reade Advanced Materials Wood's Metal Alloy (Sn + Pb + Bi + Cd) Description: A low melting fusible alloy.Various granulations are available. Used in heating baths in laboratories, antifriction metals, and solders.Information provided by Reade Advanced Materials.. |