Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.167 J/g-°C | 0.0399 BTU/lb-°F | Solid |
Indium Corp. Indalloy 217-440 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Specific Heat Capacity | 0.167 J/g-°C | 0.0399 BTU/lb-°F | Solid |
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation. |
|||
Specific Heat Capacity | 0.167 J/g-°C | 0.0399 BTU/lb-°F | Solid |
Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy Good low melting point solder for electronics assembly of for applications where Cd and Pb are to be avoided, and for thermo-electric applications. Shear rate sensitive.Information provided by the m.. |
|||
Specific Heat Capacity | 0.167 J/g-°C | 0.0399 BTU/lb-°F | Solid |
Indium Corp. Indalloy 104 Tin-Lead Solder Alloy Widely used electronic solder. Good for silver metallization. Has improved strength and fatigue propertiesInformation Provided by Indium Corporation |
|||
Specific Heat Capacity | 0.167 J/g-°C | 0.0399 BTU/lb-°F | Solid |
Indium Corp. Indalloy® 136 Bi-In-Pb-Sn Fusible Alloy General purpose fusible alloy. Wettability not outstanding. For use as solder.Information provided by the manufacturer, Indium Corporation. |
|||
Specific Heat Capacity | 0.167 J/g-°C | 0.0400 BTU/lb-°F | Liquid |
AIM 70 Fusible Alloy Uses: punch and die in short run sheet metal forming; external and internal support for bending tubing extrusions; holding jet engine blades for machining and broaching; annealing and nitriding seal.. |
|||
Specific Heat Capacity | 0.167 J/g-°C | 0.0400 BTU/lb-°F | Solid |
AIM 70 Fusible Alloy Uses: punch and die in short run sheet metal forming; external and internal support for bending tubing extrusions; holding jet engine blades for machining and broaching; annealing and nitriding seal.. |
|||
Specific Heat Capacity | 0.167 J/g-°C | 0.0399 BTU/lb-°F | Liquid |
Indium Corp. Indalloy 39 Bismuth Solder Alloy Low temperature eutectic solder. Can be used on the same metallization as SnPb based solders. Lowest temperature solder pasteInformation Provided by Indium Corporation |