Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.151 J/g-°C | 0.0361 BTU/lb-°F | Solid |
Indium Corp. Indalloy 39 Bismuth Solder Alloy Low temperature eutectic solder. Can be used on the same metallization as SnPb based solders. Lowest temperature solder pasteInformation Provided by Indium Corporation |
|||
Specific Heat Capacity | 0.151 J/g-°C | 0.0361 BTU/lb-°F | |
Mateck Thallium Bromoiodide TIBr-TII (KRS-5) Optical crystals |