Thermal Properties Metric English Comments
Specific Heat Capacity 0.580 J/g-°C

@Temperature 500 °C
0.139 BTU/lb-°F

@Temperature 932 °F
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel
Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr..
Specific Heat Capacity 0.580 J/g-°C

@Temperature 500 °C
0.139 BTU/lb-°F

@Temperature 932 °F
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be..
Specific Heat Capacity 0.580 J/g-°C

@Temperature 500 °C
0.139 BTU/lb-°F

@Temperature 932 °F
Outokumpu 353MA® High Temperature Austenitic Stainless Steel
Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but..
Specific Heat Capacity 0.580 J/g-°C
0.139 BTU/lb-°F
Premix Thermoplastics PRETHERM TPE 1050 Thermoplastic Elastomer, Boron Nitride / SEBS compound
PRETHERM TPE 1050 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It is used as gap filler between processor and heat sink or co-mold..
Specific Heat Capacity 0.580 J/g-°C
0.139 BTU/lb-°F
Schott N-SSK2 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.582 J/g-°C

@Temperature 649 °C
0.139 BTU/lb-°F

@Temperature 1200 °F
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy
Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening..