Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.1208 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.5055 J/g-°C

@Temperature 50.0 - 100 °C
0.1208 BTU/lb-°F

@Temperature 122 - 212 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed
Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 4..
Specific Heat Capacity 0.5055 J/g-°C

@Temperature 50.0 - 100 °C
0.1208 BTU/lb-°F

@Temperature 122 - 212 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 15% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
Specific Heat Capacity 0.5055 J/g-°C

@Temperature 50.0 - 100 °C
0.1208 BTU/lb-°F

@Temperature 122 - 212 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 0% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
Specific Heat Capacity 0.5055 J/g-°C

@Temperature 50.0 - 100 °C
0.1208 BTU/lb-°F

@Temperature 122 - 212 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 10% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
Specific Heat Capacity 0.5055 J/g-°C

@Temperature 50.0 - 100 °C
0.1208 BTU/lb-°F

@Temperature 122 - 212 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 20% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
Specific Heat Capacity 0.5055 J/g-°C

@Temperature 50.0 - 100 °C
0.1208 BTU/lb-°F

@Temperature 122 - 212 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 25% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..
Specific Heat Capacity 0.5055 J/g-°C

@Temperature 50.0 - 100 °C
0.1208 BTU/lb-°F

@Temperature 122 - 212 °F
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 30% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..