Polymer Property : Specific Heat Capacity = 0.0939 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.393 J/g-°C

@Temperature 20.0 °C
0.0939 BTU/lb-°F

@Temperature 68.0 °F
California Fine Wire Nico Copper Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.