Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 665 °C | 1230 °F | |
Ferro EG 0026 Glaze and Sealant Glass Glass Type: Ca-B-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insul.. |