Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 350 °C | 662 °F | |
Ferro EG 2759 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
Annealing Point | 350 °C | 662 °F | |
Ferro EG 2805 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |