Thermal Properties Metric English Comments
Annealing Point 500 °C
932 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Schott Glass 8250 Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, low refractive index, good insulator X-ray tubes, transmitting tubes, image amplifier tubes, He-Ne-lase..