Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Annealing Point 480 °C
896 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Schott Glass 8242 Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, low refractive index Clad tube for optical fibers, glass metal sealing The heavy metal content for the..
Annealing Point 480 °C
896 °F
Schott S8808 Contrast Enhancement Filter
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.