Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 462 °C | 864 °F | |
Corning 9013 Alkali Barium Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Used for sealing and other applications.Information provided by Corning Incorporated. |