Polymer Property : Annealing Point = 427 °C
Polymer Property :
Annealing Point =
427 °C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Annealing Point
427
°C
801
°F
Corning 8870 Potash Lead Crushed Glass
Used for sealing and other applications.Information provided by Corning Incorporated.