Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 420 °C | 788 °F | |
Ferro EG 2739 Thick Film Glass Glass Type: Pb-Zn-B Typical Powder Form: MVG Typical Application: Resistor Overglaze Ferro produces standard and custom glass products that are used in thick film compositions including resistors, .. |