Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 1005 °C | 1841 °F | |
Corning Vycor® 7921 UV-Blocking Neodymium Blue Glass Absorbs yellow and UV wavelengths through a process that introduces neodymium and cerium to the glass. Because the elements that create higher color temperature and UV blocking are a art of the gla.. |