Thermal Properties Metric English Comments
Annealing Point 630 °C
1170 °F
Ferro EG 2778 Thick Film Glass
Glass Type: Si-Al-Ca Typical Powder Form: MVG Typical Application: Dielectric Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct..