Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 93.3 °C | 200 °F | ASTM Test |
Lubriplate 130-A Calcium Type Multi-Purpose Grease These water resistant calcium type greases are designed for plain bearings, cams, slides, and other light-duty applications where temperatures do not exceed 170°F. See special applications. Appli.. |