Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 371 °C | 700 °F | ASTM Test |
Lubriplate SYNX HD-2 Calcium Sulfonate Complex Multi-Purpose Grease A high performance, multi-purpose, synthetic calcium sulfonate complex grease. It delivers outstanding shear stability, excellent anti-wear (AW), and extreme pressure protection. It is highly water .. |
|||
Dropping Point | 371 °C | 700 °F | ASTM Test |
Lubriplate SYNXTREME FG-2 Calcium Sulfonate Complex Synthetic Food Machinery Grade Grease A NSF H-1 registered, high performance, multi-purpose, synthetic, food machinery grade grease. Provides long lasting, anti-wear and extreme pressure protection. It is highly resistant to water and c.. |