Dropping Point 65.0 - 78.0 °C
149 - 172 °F
Struktol TPW 613 Processing Additive
STRUKTOL® TPW 613 is a functional lubricant package designed to provide superior filler wetting and dispersion characteristics in a wide range of polymer systems. This product has been engineered..