Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 274 °C | 525 °F | ASTM D-2265 |
ConocoPhillips Syncon® EP Heavy Duty Grease NLGI 2 Description: Conoco Syncon EP Heavy Duty Grease is an ultra high-performance synthetic base oil, lithium-complex grease specifically designed for extreme loading conditions. The combination of high-.. |