Thermal Properties Metric English Comments
Dropping Point >= 225 °C
>= 437 °F
ASTM D566, ISO2176
Chesterton 785 FG Parting Lubricant
Description: Chesterton® 785 FG Parting Lubricant represents the newest generation of food and pharmaceutical anti-seize compounds. A white soft-paste, formulated with proprietary blend of ultra-fi..