Thermal Properties Metric English Comments
Dropping Point 210 °C
410 °F
ASTM Test
Lubriplate FGL-00 Aluminum Complex USP Mineral Oil-Based Food Machinery Grade Grease
High performance, multi-purpose food grade grease designed to meet the demands of food and beverage industry plant engineers who want Class H-1 greases to totally replace H-2 greases. Fortified with..
Dropping Point >= 210 °C
>= 410 °F
Dow Corning MOLYKOTE® 7325 GREASE
Silicone grease especially for overrunning clutches in starter motorsInformation provided by Dow Corning
Dropping Point 210 °C
410 °F
Dow Corning MOLYKOTE® 822M GREASE
Phenyl-methyl silicone grease for automotive brake boostersInformation provided by Dow Corning
Dropping Point >= 210 °C
>= 410 °F
Dow Corning MOLYKOTE® AS-828 GREASE
Silicone grease with wide service temperature rangeInformation provided by Dow Corning