Polymer Property : Dropping Point = 367 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 186 °C
367 °F
ChevronTexaco Dura-Lith® NLGI 1 Grease EP
FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic..
Dropping Point 186 °C
367 °F
ChevronTexaco Multifak® EP NLGI Grade 1
Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec..