Polymer Property : Dropping Point = 280 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 138 °C
280 °F
ASTM Test
Lubriplate FML 0 Anhydrous Calcium USP Mineral Oil-Based Food Machinery Grade Grease
These white, multi-purpose greases have been popular in the food processing industry for years. Available in three NLGI densities for a wide variety of applications.FML Series greases are available ..
Dropping Point 138 °C
280 °F
ASTM Test
Lubriplate TEMP LOW Anhydrous Calcium Multi-Purpose Grease For Special Conditions
Multi-purpose, anhydrous calcium based grease for cold temperature applications down to -60°F. Applications: Cold temps., multi-purpose, fifth wheels. LOW TEMP is available in Cartridges, Tubes, ..