Polymer Property : Dropping Point = 265 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 265 °C
509 °F
ChevronTexaco Delo® NLGI 2 Grease EP
FeaturesChevron Delo Greases EP are technically advanced, extreme pressure greases for a wide variety of on- and off-road applications.They are formulated with ISOSYN® base stocks, a lithium comple..
Dropping Point 265 °C
509 °F
ChevronTexaco Ulti-Plex® NLGI 1 Greases EP
FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The..
Dropping Point 265 °C
509 °F
ChevronTexaco Ulti-Plex® NLGI 2 Greases EP
FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.The..