Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 226 °C | 439 °F | |
Dow Corning MOLYKOTE® 33 EXTREME LOW TEMPERATURE BEARING GREASE, LIGHT Phenyl-methyl silicone grease for extreme low temperaturesInformation provided by Dow Corning |
|||
Dropping Point | 226 °C | 439 °F | |
Dow Corning MOLYKOTE® 33 EXTREME LOW TEMPERATURE BEARING GREASE, MEDIUM Phenyl-methyl silicone grease for extreme low temperaturesInformation provided by Dow Corning |