Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 105 - 120 °C | 221 - 248 °F | |
Struktol VC-100 PVC Lubricant Package An optimized blend of special waxes and oleo chemicals.STRUKTOL® VC 100 is a formulated internal/external lubricant package. It is intended to replace paraffin wax, calcium stearate, oxidized pol.. |