Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 98.9 °C | 210 °F | ASTM Test |
Lubriplate 115 Calcium Type Multi-Purpose Grease These water resistant calcium type greases are designed for plain bearings, cams, slides, and other light-duty applications where temperatures do not exceed 170°F. See special applications. Appli.. |
|||
Dropping Point | 99.0 °C | 210 °F | |
ChevronTexaco 904 Grease NLGI Grade 1/2 Texaco 904 Grease is a calcium soap grease. It contains graphite which enhances its lubricity.Typical test data are average values only. Minor variations which do not affect product performance are .. |