Polymer Property : Dropping Point = 200 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 200 °C
392 °F
ConocoPhillips SUPER-STA NLGI No. 1
Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C...
Dropping Point 200 °C
392 °F
ConocoPhillips Syncon® HP Synthetic Grease NLGI No. 1
Description: Conoco Syncon HP Synthetic Grease is a high-quality, synthetic polyalphaolefin (PAO) lithium grease developed to provide exceptional protection and corrosion resistance for bearings and..
Dropping Point 200 °C
392 °F
ELM® SoyGrease™ HiTemp Biodegradable Extreme Pressure Grease, NLGI Grade 3
Description: ELM SoyGrease™ HiTemp grease is a premium quality biodegradable, Biotechbased™ grease formulated with OptiBase™ Oils, lithium-based thickener and extreme pressure additives for maxim..
Dropping Point 200 °C
392 °F
ASTM D2265
ExxonMobil Mobilgrease 27
Mobilgrease 27 is a high performance, aviation grease designed to combine the unique features of a synthetic ester base fluid with a lithium soap thickener. Its consistency is between an NLGI No. 1 ..
Dropping Point 200 °C
392 °F
ASTM D2265
ExxonMobil Mobilgrease 27
Mobilgrease 27 is a high performance, aviation grease designed to combine the unique features of a synthetic ester base fluid with a lithium soap thickener. Its consistency is between an NLGI No. 1 ..