Polymer Property : Dropping Point = 171 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 171 °C
340 °F
ChevronTexaco Multifak® EP NLGI Grade 0
Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec..
Dropping Point 171 °C
340 °F
ChevronTexaco Dura-Lith® NLGI 0 Grease EP
FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic..
Dropping Point 171 °C
340 °F
ASTM Test
Lubriplate MAG-00 Lithium-Polymer Type Grease For Special Applications / Conditions
These multi-purpose, lithium polymer greases have a wide operating temperature range for a variety of applications from -60°F to 300°F. Applications: Centralized systems, leaking gearboxes. MAG-00..