Dropping Point 76.7 °C
170 °F
ASTM Test
Lubriplate 105 Calcium Type Multi-Purpose Grease
These water resistant calcium type greases are designed for plain bearings, cams, slides, and other light-duty applications where temperatures do not exceed 170°F. See special applications. Appli..