Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dropping Point = 160 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 160 °C
320 °F
ChevronTexaco Dura-Lith® NLGI 000 Grease EP
FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic..
Dropping Point 160 °C
320 °F
ChevronTexaco Dura-Lith® NLGI 00 Grease EP
FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic..