Polymer Property : Dropping Point = 154 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 114 - 154 °C
237 - 309 °F
Struktol TPW 609 Processing Additive
Blend of complex, modified fatty acid ester.Applications: STRUKTOL® TPW 609 has shown excellent results in producing extruded polymer / wood composites with or without coupling agents at a lower ..