Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 140 °C | 284 °F | |
Lubriplate 777 NO. Specialty Lubricant and Grease This special grease lubricant has been approved by Ford Motor Co. specification ESF-M1C-26-A for use as a starter motor shaft lubricant. Also approved for starter drives on Evinrude / Johnson outboa.. |