Polymer Property : Dropping Point = 127 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 117 - 127 °C
243 - 261 °F
Struktol ZINC STEARATE
STRUKTOL® Zinc Stearate is one of the most widely used additives in the plastics field. It serves primarily as a lubricant, but also as a densifying agent and a partitioning agent. It is used ext..
Dropping Point 117 - 127 °C
243 - 261 °F
Struktol ZINC STEARATE CM
A clear melt zinc stearate, is manufactured from high quality stearic acid in a tightly controlled production operation that guarantees product uniformity.STRUKTOL® Zinc Stearate CM, a clear melt..
Dropping Point 117 - 127 °C
243 - 261 °F
Struktol ZINC STEARATE VG
Manufactured from high quality vegetable fatty acid with a low iodine value in a tightly controlled production operation.STRUKTOL® Zinc Stearate VG is one of the most widely used additives in the..