Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 537 - 833 °C | 999 - 1530 °F | |
PEAK Werkstoff DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT)abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of p.. |