Thermal Properties Metric English Comments
Melting Point 900 - 915 °C
1650 - 1680 °F
Wieland 1914 Wilaform Gold
Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental