Melting Point 880 - 900 °C
1620 - 1650 °F
Wieland 1605 Wilaform Gold
Red gold for all kinds of decoration manufacturing.Applications: casting, laminar decoration, pipes, tubingDental
Melting Point 800 - 900 °C
1470 - 1650 °F
Wieland 3012 Wilaform Silver
A balance of manufacturing and performance characteristics makes this the preferential silver alloy in the decoration manufacturing industry. The alloy unites good ductility properties with the nec..
Melting Point 850 - 900 °C
1560 - 1650 °F
Williams Advanced Alloys Wambraze™ WB900B Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..