Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 470 °C | 878 °F | |
Oceanchem Group Ethylenebistetrabromophthalimide (BT93W) Molecular Formula: C18H4N2O4Br8Cas No.: 32588-76-4Features: White color, outstanding thermal and UV stability, non-blooming, excellent wet electrical properties.Applications: Use in polyolefins, hig.. |