Polymer Property : Melting Point = 840.6 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 840.6 - 879.4 °C
1545 - 1615 °F
Lucas-Milhaupt BRAZE 051 Silver Based Cadmium Free Filler Metal
Characteristics:Braze 051 is a low cost, intermediate temperature silver brazing filler metal suitable for joining various ferrous and non-ferrous alloys that can be heated to 1650EF/900EC without d..