Thermal Properties Metric English Comments
Melting Point 824 - 853 °C
1520 - 1570 °F
Williams Advanced Alloys Wambraze™ WB853 Solder
High-purity vacuum cast materials are manufactured by Williams in a variety of solder alloys, including gold brazing alloys for electronic packaging and high temperature joining vacuum electronic de..
Melting Point 824 °C
1520 °F
American Elements Ytterbium Nanoparticles
General DescriptionYtterbium (Yb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Ytterbium Particles are typically 10 - 80 nanometers (nm) with spec..